rain erosion

Testing conditions

If an opening occurs earlier in the test schedule than originally confirmed and the coated specimens are received, the test will be run unless otherwise agreed with the customer.

During the RE test the specimens are exposed to a very large quantity of water. This water have an influence on the weight of the specimen during the test. Hence, the weight of the specimen during the test period will not reflect the loss in mass during test. Therefore, the weight is not recorded during the test.

By customer manufactured specimens the customer is liable for any damages resulting from accidents caused by the specimens.

Contact

PolyTech A/S

Industrivej 37
DK-6740 Bramming
Denmark